Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.40 J/cm² @Temperature -30.0 °C |
35.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Charpy Impact Unnotched | 7.40 J/cm² @Temperature 23.0 °C |
35.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT Description: Is a PBT-I, injection-molding grade with 30% glass fibers, for rigid, tough and dimensionally stable technical parts with increased requirements on hydrolysis resistance and toughness, .. |