Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 13.3 J/cm² @Temperature -30.0 °C |
63.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 13.3 J/cm² @Temperature 23.0 °C |
63.3 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |