Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.10 - 1.30 J/cm²

@Temperature 23.0 °C
5.24 - 6.19 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
Charpy Impact Unnotched 1.10 J/cm²

@Temperature -20.0 °C
5.24 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 1.10 J/cm²

@Temperature -40.0 °C
5.24 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 1.10 J/cm²

@Temperature 23.0 °C
5.24 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Inno-Comp INNOPOL® CS 1-2140 BLH 40% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-2140 BLH is recommended especially for producing products, where high stiffness, low shrinkage, long term heat stability and excellent processability are required.All information pr..