Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 86.0 J/cm² @Temperature -30.0 °C |
409 ft-lb/in² @Temperature -22.0 °F |
PB; ISO 179/1eU |
Inno-Comp INNOPOL® CS 2-9000 MA N Polypropylene Copolymer INNOPOL® CS 2-9000 MA N is a high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA N is developed for producing injection molded automotive components.All information provide.. |