Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.500 - 0.700 J/cm²

@Temperature 23.0 °C
2.38 - 3.33 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Charpy Impact Unnotched 0.400 - 0.700 J/cm²

@Temperature -40.0 °C
1.90 - 3.33 ft-lb/in²

@Temperature -40.0 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
Charpy Impact Unnotched 0.450 - 0.700 J/cm²

@Temperature 23.0 °C
2.14 - 3.33 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..