Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.28 J/cm²

@Temperature -30.0 °C
20.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Crastin® CE15330 BK010 PBT  (Unverified Data**)
Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..