Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 39.0 J/cm² @Temperature 23.0 °C |
186 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |