Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.10 J/cm² @Temperature -20.0 °C |
14.8 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 T 40 FRO 3 PA66, 40% mineral filling, flame retardant FeaturesPA 66 with the content of 40% chemically modified mineral filling a with fire retardant. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produ.. |
|||
Charpy Impact Unnotched | 3.10 J/cm² @Temperature -20.0 °C |
14.8 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 T 40 Polyamide 66, 40% Mineral Filled FeaturesPA 66 with the content of 40% chemically modified mineral filling. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cov.. |
|||
Charpy Impact Unnotched | 3.10 J/cm² @Temperature -30.0 °C |
14.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
PolyOne Bergamid™ B65 G/Mi20 UF grey LS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 3.10 J/cm² @Temperature 23.0 °C |
14.8 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
PolyOne Bergamid™ B70 GK/Mi30 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 3.10 J/cm² @Temperature -30.0 °C |
14.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Charpy Impact Unnotched | 3.10 J/cm² @Temperature -30.0 °C |
14.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |