Polymer Property : Charpy Impact Unnotched = 124 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 26.0 J/cm²

@Temperature 0.000 °C
124 ft-lb/in²

@Temperature 32.0 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior..
Charpy Impact Unnotched 26.0 J/cm²

@Temperature 23.0 °C
124 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® N2320 0035 LEV POM
Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF
Charpy Impact Unnotched 26.0 J/cm²

@Temperature 23.0 °C
124 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® N2320 006 POM
Description: Is a POM, high-molecular-weight grade with somewhat increased flowability for injection molding of relatively thick-walled moldings.Information provided by BASF
Charpy Impact Unnotched 26.0 J/cm²

@Temperature 23.0 °C
124 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® N2320 0035 POM
Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF