Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
PolyOne Bergamid™ A70 GK30 black 13539126 Polyamide 66 (Nylon 66) Information provided by PolyOne |