Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 5.09788 - 5.09788 J @Temperature -30.0 - -30.0 °C |
3.76000 - 3.76000 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 5.10 J Grade Count:1 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Falling Dart Impact | 5.09788 - 5.09788 J @Thickness 1.78 - 1.78 mm |
3.76000 - 3.76000 ft-lb @Thickness 0.0701 - 0.0701 in |
Average value: 5.10 J Grade Count:1 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |