Polymer Property : Modulus of Rigidity = 71.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rigidity 0.490 GPa
71.1 ksi
ASTM-D747
Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer
IF33 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, good flexibility, ..