Mechanical Properties Metric English Comments
Modulus of Rigidity 82.7 GPa
12000 ksi
Latrobe Lescalloy® 52100 VAC-ARC High Performance Bearing Steel
LESCALLOY 52100 VAC-ARC is a deep hardening alloy steel used for aircraft bearings and other high stressed parts where good rolling contact fatigue strength is required at operating temperatures bel..