Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TD2 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TDX Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TH1 Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TH1 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TH2 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TH3 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TH4 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 THX Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 THX Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TD1 Rod quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TD1 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TD3 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Modulus of Rigidity | 115 GPa | 16700 ksi | Torsion |
CLAL-MSX DECLAFOR® 1015 TF Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |