Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.586 MPa @Strain 100 % |
85.0 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Uniprene® UN-2012-L3 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |