Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 82.0 MPa | 11900 psi | |
Lehmann & Voss LUVOCOM® 1301-7294/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Tensile Stress | 82.0 MPa | 11900 psi | |
Lehmann & Voss LUVOCOM® 50-7224/V0 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Improved f.. |