Polymer Property : Tensile Stress = 8.27 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 8.27 MPa

@Strain 300 %
1200 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1538A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 8.27 MPa

@Strain 300 %
1200 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2103 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 8.27 MPa

@Strain 300 %
1200 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-4145A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..