Polymer Property : Tensile Stress = 7.17 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 7.17 MPa

@Strain 100 %
1040 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer
A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard..