Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 46.0 MPa | 6670 psi | |
Lehmann & Voss LUVOCOM® 80/TF/18/GY Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Tensile Stress | 46.0 MPa | 6670 psi | |
Lehmann & Voss LUVOCOM® 80/TF/18/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |