Polymer Property : Tensile Stress = 61.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 61.0 MPa
8850 psi
Lehmann & Voss LUVOCOM® 20-7314 Polyphthalamide, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..