Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.20 MPa @Strain 10.0 % |
609 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® G4078LS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Light ProtectionInformation provided by DuPont Performance Polymers |