Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.62 MPa @Strain 300 %, Temperature 23.0 °C |
960 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7990-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-1001-00 can be re.. |
|||
Tensile Stress | 6.62 MPa @Strain 300 %, Temperature 23.0 °C |
960 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7990-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-9001-02 can be re.. |