Mechanical Properties Metric English Comments
Tensile Stress 58.0 MPa
8410 psi
Lehmann & Voss LUVOCOM® 1700-8126 PPO, with glass spheres and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..