Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 56.0 MPa | 8120 psi | |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Tensile Stress | 56.0 MPa | 8120 psi | |
Lehmann & Voss LUVOCOM® 80-8444 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.dynamic stressReduced moment of inertia compared with metal parts.Isotropic shrinkage character.. |