Polymer Property : Tensile Stress = 5220 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 36.0 MPa
5220 psi
at Break; ISO 527
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene
EX 6HT is a high density polyethylene with 1-Butene as co monomer. It has good toughness, low gel level, good tear strength, high tenacity.Applications: film extrusion, blending partner, refuse ba..
Tensile Stress 36.0 MPa
5220 psi
at Break; ISO 527
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene
EX3-100S is a high density polyethylene with 1-Butene as co monomer. It is natural, outstanding ESCR, high impact strength, outstanding hydrostatic strength for PE 100 class.Applications: pipe extr..