Mechanical Properties Metric English Comments
Tensile Stress 3.52 MPa

@Strain 300 %
511 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL 0117-5 NATURAL Styrene Butadiene Block Copolymer (SBC)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..