Polymer Property : Tensile Stress = 5.80 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 5.80 MPa

@Strain 100 %
841 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 9221-87 Thermoplastic Vulcanizate
Product Description: A hard, colorable UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resista..