Mechanical Properties Metric English Comments
Tensile Stress 3.43 MPa

@Strain 100 %
498 psi

@Strain 100 %
ASTM D412
Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..