Mechanical Properties Metric English Comments
Tensile Stress 2.60 MPa

@Strain 100 %,
Temperature 23.0 °C
377 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE)
Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC..
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-70B230 Thermoplastic Elastomer
A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner ..
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 121-70M350 Thermoplastic Vulcanizate - UV Resistant
Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for gap filler applications requiring scratch..
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those..
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 241-64 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for..