Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 25.2 MPa | 3650 psi | At break; ISO 527 |
FKuR Kunststoff Terralene® WF 3516 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |