Polymer Property : Tensile Stress = 3480 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 24.0 MPa
3480 psi
50 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 2-7120 20% Talc Filled Polypropylene Copolymer
INNOPOL® CS 2-7120 is a 20 % talc-filled polypropylene block-copolymer compound /PP-B TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-7120 is recomme..
Tensile Stress 24.0 MPa
3480 psi
Lehmann & Voss LUVOCOM® 100-7126 VP Thermoplastic polyurethane, with PTFE
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K..