Tensile Stress 315 MPa
45700 psi
Lehmann & Voss LUVOCOM® 20-0951 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..