Polymer Property : Tensile Stress = 3050 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 21.0 MPa
3050 psi
50 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 2-2523 EP 16% Talc Filled, Elastomer Modified Polypropylene Copolymer
INNOPOL® CS 2-2523 EP is a 16% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in natural and custom colored form.INNOPOL® CS 2-2523 EP..