Polymer Property : Tensile Stress = 3.30 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.30 MPa

@Strain 100 %
479 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-80B230 Thermoplastic Elastomer
A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner ..