Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.20 MPa @Strain 100 % |
464 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 291-75B150 Thermoplastic Vulcanizate Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app.. |