Polymer Property : Tensile Stress = 2760 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 19.0 MPa

@Strain 1.00 %,
Time 3.60e+6 sec
2760 psi

@Strain 1.00 %,
Time 1000 hour
DIN 53444
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..