Tensile Stress 20.0 MPa
2900 psi
Lehmann & Voss LUVOCOM® 65-8498 PP-copolymer, unreinforced
Applications: Office communication.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable for thin wall complex parts.Information provided by Lehmann & Voss &..