Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.76 MPa @Strain 300 %, Temperature 23.0 °C |
400 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |
|||
Tensile Stress | 2.76 MPa @Strain 300 %, Temperature 23.0 °C |
400 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2755C Thermoplastic Elastomer (TPE) Dynaflex™ G2755C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypropylene .. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1085 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1097D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1504L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1504-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1518C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1564-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1564L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1564L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1646-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1657L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1665-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1791R4 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1838-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2120 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2132 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2260 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2260-R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1855J Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2770L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2850M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-1424A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 2.76 MPa @Strain 100 % |
400 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-87-L832A Thermoplastic Elastomer Notes: UV Stabilized Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstrip.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2850M L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1037 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2770 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2850M-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |