Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.70 MPa @Strain 100 % |
392 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KG 70A-3S2019 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Stress | 2.70 MPa @Strain 100 % |
392 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 691-65W175 Thermoplastic Vulcanizate Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for thin wall, architectural glazing and sealing applic.. |
|||
Tensile Stress | 2.70 MPa @Strain 100 % |
392 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Tensile Stress | 2.70 MPa @Strain 100 % |
392 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 191-70PA Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft .. |