Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1181 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1249B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1580 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1580D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1580L1-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1580-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1586 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1695L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1743UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1775 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1775A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1776A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1829-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2207B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 100 % |
300 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Monprene® MP-2302 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1349A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1876 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2745 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2750L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2760 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2760BR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2840M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2850E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-3017 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-1295B Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Soft Touch Applications; Flexible Grips; Handles; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: M.. |
|||
Tensile Stress | 2.07 MPa @Strain 100 % |
300 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Uniprene® UN-7010-55NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2750 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.07 MPa @Strain 300 % |
300 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-3005 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |