Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 158 MPa | 22900 psi | |
Lehmann & Voss LUVOCOM® 20-8254 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Tensile Stress | 158 MPa | 22900 psi | |
Lehmann & Voss LUVOCOM® 1104-7598 Polyether ketone, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str.. |