Polymer Property : Tensile Stress = 155 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 155 MPa
22500 psi
Lehmann & Voss LUVOCOM® 1105-8350 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Tensile Stress 155 MPa
22500 psi
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Tensile Stress 155 MPa
22500 psi
Lehmann & Voss LUVOCOM® 1-7395 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R..
Tensile Stress 155 MPa
22500 psi
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
Tensile Stress 155 MPa
22500 psi
Lehmann & Voss LUVOCOM® 20-8114 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Tensile Stress 155 MPa
22500 psi
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Tensile Stress 155 MPa
22500 psi
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
Tensile Stress 155 MPa
22500 psi
Lehmann & Voss LUVOCOM® 1-7943 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Tensile Stress 155 MPa
22500 psi
ISO 527-2
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs..
Tensile Stress 155 MPa
22500 psi
ISO 527-2
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S..