Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 15.7 MPa @Strain 100 % |
2280 psi @Strain 100 % |
ASTM D412 |
Kolon ELLAS K-260D Thermoplastic Polyurethane ApplicationsExtrusion: Antenna, Heel TipInjection: Hose, Tube, SheetIndustry Parts Information provided by API-Kolon. |
|||
Tensile Stress | 15.7 MPa | 2280 psi | at Break, MD; ASTM D882 |
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene LF0200 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. LF0200 contains antioxidant.Applications: genera.. |