Polymer Property : Tensile Stress = 145 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.00 MPa

@Strain 100 %
145 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer
A soft, black, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/PS b..
Tensile Stress 1.00 MPa

@Strain 100 %
145 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Tensile Stress 1.00 MPa

@Strain 100 %
145 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/..