Mechanical Properties Metric English Comments
Tensile Stress 9.81 MPa

@Strain 100 %
1420 psi

@Strain 100 %
ASTM D412
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon.
Tensile Stress 9.81 MPa

@Strain 100 %
1420 psi

@Strain 100 %
ASTM D412
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane
ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.