Polymer Property : Tensile Stress = 1280 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 8.83 MPa

@Strain 100 %
1280 psi

@Strain 100 %
ASTM D412
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusion: Cable Sheathing, high pressure tubeInjectionElectric WireIndustry Parts Information provided by API-Kolon.