Mechanical Properties Metric English Comments
Tensile Stress 77.0 MPa
11200 psi
Lehmann & Voss LUVOCOM® 1105-7198/BK PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..