Polymer Property : Tensile Stress = 10.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 10.8 MPa

@Strain 100 %
1560 psi

@Strain 100 %
ASTM D412
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane
ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon.