Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.80 MPa @Strain 100 % |
261 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 101-55W255 Thermoplastic Vulcanizate Product Description: A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for use in residential dishwasher applications and contains.. |