Polymer Property : Tensile Strength at Break = 9990 psi
Polymer Property :
Tensile Strength at Break =
9990 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
51.7
-
68.9
MPa
7500
-
9990
psi
ASTM D638
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer